PLA材质配件耐温性差,玻璃化温度约55-60℃,遇烘干机高温或夏季车内暴晒会软化变形,需机洗烘干的日常服装不建议用纯PLA纽扣
1
Sources
80%
Confidence
Long-term
Relevance
-
First Seen
Sources
Related Entities
Related Claims
UnverifiedPLA材质耐热性差,环境温度超过约55-60°C时材料会软化变形,不适合需要在高温仓储或夏季暴晒环境下长期存放的包裹防护88% similarUnverified不适合用于需要机洗高温程序(60℃以上)或烘干机烘干的服装,PLA材质在高温下易变形软化85% similarUnverifiedPLA+PBAT复合材质降解袋适合常温干货,但耐温仅约50-60℃,装刚出锅的热食或高温环境下会软化变形;需装热食应选专门标注耐高温的PLA吸管级材质82% similarUnverified夏季车内暴晒温度可达60-70℃,不建议选纯双面胶固定的挂钩挂重物,高温胶体软化易整体脱落砸落物品80% similarUnverified隔热垫材质需关注耐温标称,PVC/普通泡棉在夏季暴晒下(仪表台可达70-80℃)易释放异味或软化变形,聚酯纤维+铝箔复合材质耐温性和低气味表现更好80% similar