The brittleness of stone means that too deep a cut during rough machining can cause chipping or propagate internal cracks, while too fast a feed during finishing can cause surface spalling, so the parameter window for stone CNC is much narrower than for metal and requires operators to experiment repeatedly according to the specific type of stone.